ITEM PROPERTY |
Corundum-Spinel Castable HXCMA-93 |
MgO-Cr2O3 Ramming Mix HXMGE-55 |
MgO Gunning Refractory Mix HXMC-80 |
MgO-Cr2O3 Refractory Mortar HXMGE-50 |
|
---|---|---|---|---|---|
Al2O3 % ≥ |
85 |
/ |
/ |
/ |
|
MgO % ≥ |
8 |
55-60 |
83 |
50 |
|
Cr2O3 % ≥ |
/ |
16 |
/ |
18 |
|
SiO2 % ≤ |
/ |
1.5 |
/ |
/ |
|
B. D. g/cm3 ≥ (110℃×24h) |
3.0 |
3.10 |
2.30 |
/ |
|
C. C. S. (MPa)≥ |
110℃×24h |
30 |
30 |
5 |
1.5 |
1500℃×3h |
80 |
40 |
20 |
1.0 |
|
M.O.R (MPa)≥ |
110℃×24h |
5 |
5 |
2 |
/ |
1500℃×3h |
10 |
6 |
5 |
/ |
|
P.L.C (%) |
1500℃×3h |
0--1.0 |
-0.5--+0.5 |
-1.5--+3.0 |
Bonding time: 1-3 min |
*They are typical values in this table, not a basis for order.